Why Do Crease Lines Crack on Double Wall Board
- Category: Company News
- Author: Xinshida
- Published: 2026-11-26 10:10:32
- Views: 151
Summary: Crease cracking explained for corrugated converting equipment: working ranges, setup sequence, tolerance control and corrective action for crease cracking.
Why Do Crease Lines Crack on Double Wall Board
Summary: Crease cracking explained for corrugated converting equipment: working ranges, setup sequence, tolerance control and corrective action for crease cracking.
- Category: Company News
- Author: Xinshida
- Published: 2026-11-26 10:10:32
- Views: 151
Key Parameters and Working Ranges
The table below gives typical working values used for crease cracking on standard corrugated converting equipment. They are starting points for a setup, not acceptance limits; the limits for a given order should be taken from the job specification and the measured condition of the board being run.
Parameter | Typical working value | How it is used |
Crease width | 7 to 10 millimetres for double wall | Verify against the machine specification and the board grade in use. |
Wheel penetration | 50 to 60 percent of caliper | Measure at production speed after the line has warmed up. |
Creasing pressure | 0.6 to 0.8 megapascal | Record on the setup sheet at the start of each order. |
Pre scoring | recommended above 7 millimetre caliper | Recheck after any tooling or material change. |
Each value should be recorded together with the board grade, flute type and line speed at which it was measured. Board is a hygroscopic material, so the same setting can behave differently on a dry morning and a humid afternoon. Recording temperature and humidity alongside the setting makes the record comparable.
Working Principle Behind Crease cracking
The creasing and scoring station works within a narrow window defined by crease width and wheel penetration. When crease width is held at 7 to 10 millimetres for double wall, the process stays repeatable; as soon as the value leaves that window, the first visible sign is crease cracking. Understanding that chain of cause and effect is more useful than memorising a single number, because the correct value shifts with board grade, flute type and line speed.
Board caliper and flute direction interact with the setting, so an adjustment made to one of them should never be treated as independent. For example, a change that improves the result at low speed can behave differently at production speed, which is why the same check is repeated after the line has stabilised. Where a limit is given as a range, the lower half of the range usually gives the safer starting point for a new board grade; the setting can then be raised only after the measured result confirms that it is needed.
Consumable and Substrate Considerations
Corrugated board is not a uniform substrate. Liner finish, medium strength, caliper and moisture content all vary between lots, and each of them changes how crease cracking behaves. Two pallets of nominally identical board can need different settings, which is why crease width and wheel penetration are checked at every incoming lot rather than assumed.
Additional Practical Notes
Crease cracking is checked against the job card at the start of each order, and the reading is filed with the board grade and the line speed at which it was taken. Trial sheets used for setup are counted separately, so the true waste of a changeover stays visible in the shift figures.
Shift Level Checklist
Confirm the job recipe, the board grade and the drawing before the first sheet of crease cracking is checked.
Verify crease width against the setup sheet at the start of each shift rather than after a complaint.
Record the measured result of every first off sample so that drift can be seen across orders.
Keep crease width and wheel penetration clean and inspect them for wear at the defined interval.
Watch for crease cracking and correct one variable at a time, measuring after each change.
File the final setting, the correction made and the reason for it at handover.
Summary for the Shift
Stable crease cracking comes from a measured target, a defined tolerance and a routine that is followed on every order. Keep crease width at 7 to 10 millimetres for double wall, verify the first off sample, watch for crease cracking and record every correction. Those habits do more for output and consistency than a single large adjustment made after a complaint.
Figures quoted in this article are typical working values for standard corrugated converting equipment. They should be verified against the specification of the machine in use, the board grade being processed and the conditions measured on the shift before they are used as acceptance limits.
References
[1] ISO 12647-2:2013, Graphic technology - Process control for the production of half-tone colour separations, proof and production prints - Part 2: Offset lithographic processes.
[2] ISO 9001:2015, Quality management systems - Requirements.
[3] TAPPI T 804 om-12, Compression test of fiberboard shipping containers.
[4] TAPPI T 839 pm-13, Edgewise compressive strength of corrugated fiberboard (short column test).
[5] ASTM D642-15, Standard Test Method for Determining Compressive Resistance of Shipping Containers, Components, and Unit Loads.
[6] EN 415-1:2014, Safety of packaging machines - Part 1: Terminology and classification of packaging machines and associated equipment.
[7] IEC 60204-1:2016, Safety of machinery - Electrical equipment of machines - Part 1: General requirements.
扫二维码用手机看
Address: Dongguang County, Cangzhou City, Hebei Province, China
Phone: +86 13930771388
WhatsApp: +86 13930771388
Email: 1971637272@qq.com
Website: https://www.xinshidamfg.com
- Follow Xinshida -
Copyright © 2019 Cangzhou Xinshida Machinery Equipment Co., Ltd.