Xinshida
News
[Featured]
[Top]

Anilox Roll Cell Volume, Line Count and Ink Film Thickness Selection

  • Category: Company News
  • Author: Xinshida
  • Published: 2026-11-26 10:06:56
  • Views: 178

Summary: Anilox cell volume selection explained for corrugated converting equipment: working ranges, setup sequence, tolerance control and corrective action for density drift.

[Featured]
[Top]

Anilox Roll Cell Volume, Line Count and Ink Film Thickness Selection

Summary: Anilox cell volume selection explained for corrugated converting equipment: working ranges, setup sequence, tolerance control and corrective action for density drift.

  • Category: Company News
  • Author: Xinshida
  • Published: 2026-11-26 10:06:56
  • Views: 178
详情
Anilox cell volume selection is one of the settings that decides whether a corrugated converting line runs steadily or spends the shift being corrected. This article explains what the flexo printing unit does, which parameters govern anilox cell volume selection, how density drift develops when the setting drifts, and what to measure so that the line stays inside tolerance across a full production run. It is written for production managers, process engineers and operators who need to make a decision or fix a problem on the shift rather than read a catalogue description.

Parameters to Record on the Job Card

The table below gives typical working values used for anilox cell volume selection on standard corrugated converting equipment. They are starting points for a setup, not acceptance limits; the limits for a given order should be taken from the job specification and the measured condition of the board being run.

Parameter

Typical working value

How it is used

Cell volume for line work

4.5 to 6.0 cubic centimetres per square metre

Verify against the machine specification and the board grade in use.

Line count for solids

180 to 220 lines per inch

Measure at production speed after the line has warmed up.

Line count for fine type

300 to 360 lines per inch

Record on the setup sheet at the start of each order.

Engraving angle

60 degree hexagonal

Recheck after any tooling or material change.

Each value should be recorded together with the board grade, flute type and line speed at which it was measured. None of these adjustments should be made while the guard is open or the machine is in a powered state. Isolation, verification and a controlled restart are part of the adjustment, not an interruption to it.

Working Principle Behind Anilox cell volume selection

The flexo printing unit works within a narrow window defined by cell volume and line count. When cell volume for line work is held at 4.5 to 6.0 cubic centimetres per square metre, the process stays repeatable; as soon as the value leaves that window, the first visible sign is density drift. Understanding that chain of cause and effect is more useful than memorising a single number, because the correct value shifts with board grade, flute type and line speed.

Ink film thickness and cell geometry interact with the setting, so an adjustment made to one of them should never be treated as independent. For example, a change that improves the result at low speed can behave differently at production speed, which is why the same check is repeated after the line has stabilised. Board is a hygroscopic material, so the same setting can behave differently on a dry morning and a humid afternoon. Recording temperature and humidity alongside the setting makes the record comparable.

Diagnosing the Usual Problems

When density drift appears, the first checks are the simplest ones: confirm cell volume for line work is still at 4.5 to 6.0 cubic centimetres per square metre, confirm cell volume is clean and undamaged, and confirm the board has not changed. In most cases the fault is a setting that has drifted or a wear item at the end of its life, not a failed major component.

Additional Practical Notes

Anilox cell volume selection is checked against the job card at the start of each order, and the reading is filed with the board grade and the line speed at which it was taken. Trial sheets used for setup are counted separately, so the true waste of a changeover stays visible in the shift figures.

Shift Level Checklist

  • Confirm the job recipe, the board grade and the drawing before the first sheet of anilox cell volume selection is checked.

  • Verify cell volume for line work against the setup sheet at the start of each shift rather than after a complaint.

  • Record the measured result of every first off sample so that drift can be seen across orders.

  • Keep cell volume and line count clean and inspect them for wear at the defined interval.

  • Watch for density drift and correct one variable at a time, measuring after each change.

  • File the final setting, the correction made and the reason for it at handover.

Summary for the Shift

Stable anilox cell volume selection comes from a measured target, a defined tolerance and a routine that is followed on every order. Keep cell volume for line work at 4.5 to 6.0 cubic centimetres per square metre, verify the first off sample, watch for density drift and record every correction. Those habits do more for output and consistency than a single large adjustment made after a complaint.

Figures quoted in this article are typical working values for standard corrugated converting equipment. They should be verified against the specification of the machine in use, the board grade being processed and the conditions measured on the shift before they are used as acceptance limits.

References

  • [1] ISO 12647-2:2013, Graphic technology - Process control for the production of half-tone colour separations, proof and production prints - Part 2: Offset lithographic processes.

  • [2] ISO 9001:2015, Quality management systems - Requirements.

  • [3] TAPPI T 804 om-12, Compression test of fiberboard shipping containers.

  • [4] TAPPI T 839 pm-13, Edgewise compressive strength of corrugated fiberboard (short column test).

  • [5] ASTM D642-15, Standard Test Method for Determining Compressive Resistance of Shipping Containers, Components, and Unit Loads.

  • [6] EN 415-1:2014, Safety of packaging machines - Part 1: Terminology and classification of packaging machines and associated equipment.

  • [7] IEC 60204-1:2016, Safety of machinery - Electrical equipment of machines - Part 1: General requirements.

扫二维码用手机看

Address: Dongguang County, Cangzhou City, Hebei Province, China

Phone: +86 13930771388

WhatsApp: +86 13930771388

Email: 1971637272@qq.com

Website: https://www.xinshidamfg.com

Xinshida公众号

- Follow Xinshida -

Xinshida

Copyright © 2019 Cangzhou Xinshida Machinery Equipment Co., Ltd.